TemPro 187 V

TemPro 187 V


Datasheet
Download
Features
Category
Repair - Maintenance & Joining
Standard
-
Hardness
Yield Strength: 450 MPa; Tensile Strength: 700 MPa; Hardness: 350 HB (WH)
Microstructure
-
Dia
2.40, 3.20, 4.00 mm
Package
Plastic Box - 5 Kg
General Informations & Typical Applications

- Rutile-basic coated Ni-Cr-Mo alloyed and high recovery (170%)

- Superior resistance to creep, fatigue, cracking, scaling, corrosion, carburisation

- Stable grain structure is not embrittled by thermal shock/cycling from 1100°C

- Work hardened alloy up to 350 HB

  • Construction of gas turbines, combustion chambers, ovens, thermal equipment for heat treatment
  • Petro-chemical installation
  • Joining alloy stainless steels, nickel alloys and dissimilar metals

Wear Types
Abrasion

Impact

Metal-Metal

High Temperature

Corosion

Welding Positions: PA, PB, PC, PD, PE, PF

Current Type: DC (+)